Mechanical Properties Metric English Comments
Compressive Strength 17.9 MPa
2600 psi
Length
Pyrotek PTB 2200 Structural Board
ApplicationsCaster tips Small machined nozzles Slotted caster tips AdvantagesHigh strength Resistant to thermal shock Easily machined Non-wetting to molten non-ferrous metals Low thermal mass High t..
Compressive Strength 17.9 MPa

@Treatment Temp. 104 °C
2600 psi

@Treatment Temp. 219 °F
Cold Crush Strength; Dried 104°C
BNZ Materials Blazecrete 2600 Dense Castable
Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as..