Polymer Property : Compressive Strength = 261000 psi
Polymer Property :
Compressive Strength =
261000 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Strength
1800
MPa
261000
psi
GBC Grade 90 Alumina
Data provided by the manufacturer, GBC Materials Corporation.