Mechanical Properties Metric English Comments
Compressive Strength 2700 MPa
392000 psi
DIN 51067T1
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2
DN 70 is a ZTA Alumina Toughened Zirconia.
Compressive Strength 2700 MPa
392000 psi
Rc0.2; at HRC=62
Bohler-Uddeholm UDDEHOLM Vancron 40 nitrided powder tool steel
Description: Uddeholm Vancron 40 is a nitrided powder tool steel, which means that a “surface coating” is already integrated into the finished tooling material. The result is a tool surface with v..
Compressive Strength 2700 MPa
392000 psi
Rcm. Hardness HRC 60.
Assab Steels CALMAX Plastic Mold Material
CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo..
Compressive Strength 2700 MPa
392000 psi
ASTM C-773-88 / DIN 51067T1
CeramTec 433 Alumina, 99.9%
433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A ..