Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 2900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 14.0 - 20.0 MPa
2030 - 2900 psi
ASTM D695
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st..