Compressive Strength 202 MPa
29300 psi
ASTM D695
Greene Tweed WRâ„¢ 300 PEEK, Carbon Filled
WR®300 is a carbon-fiber reinforced compression molded PEEK often selected by pump manufacturers and users for pump bushings and case or impeller wear rings. Maximum service life is achieved in ..
Compressive Strength 202 MPa
29300 psi
ASTM D695
Plenco 1530 Polyester, Briquette, Transfer Molded
PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab..
Compressive Strength 202 MPa
29300 psi
ASTM D695
Plenco 2535 Phenolic, Granular, Injection Molded
PLENCO 02535 is a general purpose, organic filled phenolic molding compound offering optimized cure characteristics and excellent electrical properties. Type ASTM 5948 CFG, and UL recognized under c..