Mechanical Properties Metric English Comments
Compressive Strength 3.43 MPa
498 psi
Cold Crushing
Sharadaa Ceramics 29 Insulation Bricks-ASTM
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 3.43 MPa
498 psi
Cold Crushing
Sharadaa Ceramics 32 Insulation Bricks-ASTM
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 3.43 - 4.41 MPa
498 - 640 psi
Cold Crushing
Sharadaa Ceramics HFK Insulation Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..