Polymer Property : Compressive Strength = 303 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 2.09 MPa
303 psi
25 g/l
Jackon JACKOCELL® S2314 Expanded Polystyrene Construction and Block Molding
100% PolystyrenePre-expansionThis is the low pentane version for high quality block molding.Block MouldingJackocell® S2314 represents the favorite choice for the manufacture of high quality insul..