Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.228 MPa | 33.0 psi | 10% Deformation; Fired |
Unifrax Fiberfrax® Duraboard® 500ES Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |
|||
Compressive Strength | 0.228 MPa | 33.0 psi | 15% Deformation; Fired |
Unifrax Fiberfrax® Duraboard® 350ES Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |
|||
Compressive Strength | 0.228 MPa | 33.0 psi | 10% Deformation; Fired |
Unifrax Fiberfrax® Duraboard® HD Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |