Polymer Property : Compressive Strength = 3300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 22.8 MPa
3300 psi
10% Def.; ASTM D695
Quadrant EPP TIVAR® 1000 EC Electrically Conductive UHMW (ASTM Product Data Sheet)
Compressive Strength 22.8 MPa
3300 psi
10% Def.; ASTM D695
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW, Black (ASTM Product Data Sheet)
Compressive Strength 22.8 MPa
3300 psi
10% Def.; ASTM D695
Quadrant EPP TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet)
Compressive Strength 22.8 MPa
3300 psi
10% Def.; ASTM D695
Quadrant EPP TIVAR® ESD Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet)
Protects against electrical charge build-up Reduces noise Self-lubricating Corrosion-resistant No moisture absorption
Compressive Strength 22.8 MPa
3300 psi
1% strain; ASTM D695
Saint-Gobain Meldin® 7001 Isostatically Molded Polyimide
Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high ..
Compressive Strength 22.8 MPa
3300 psi
1% strain; ASTM D695
Saint-Gobain Meldin® 7211 Isostatically Molded Graphite and PTFE Filled Polyimide
Finished parts and basic shapes made from 10% by weight PTFE and 15% by weight graphite filled polyimide material for applications requiring a very low coefficient of friction and self-lubricating p..