Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 35.9 MPa | 5200 psi | ASTM D695 |
Ensinger ENSITEP® PET Polyethylene Terephthalate - Extruded Products
(discontinued **) ENSITEP is an unreinforced, semi-crystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus, and .. |
|||
Compressive Strength | 35.9 MPa | 5200 psi | |
Engineered Syntactic Systems BZ-30 Deep Water Syntactic Foam Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having.. |
|||
Compressive Strength | 35.9 MPa | 5200 psi | ASTM D695 |
Ensinger Delrin® 150 Homopolymer Acetal (POM) Ensinger's Delrin® 150 stock shapes are a homopolymer acetal manufactured using DuPont Delrin 150 Resin. It is a crystalline plastic which offers an excellent balance of properties to bridge the g.. |
|||
Compressive Strength | 35.9 MPa | 5210 psi | |
Abatron LiquidWood® Deep Penetrating Wood Consolidant LiquidWood® is a deep penetrating wood consolidant that regenerates and waterproofs rotted, dried-out, or spongy wood. It restores structural strength and durability to wood fibers. With LiquidWood.. |