Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 360 MPa | 52200 psi | ISO 604 |
Sumitomo Bakelite North America RX® 630 Fiberglass Reinforced Phenolic RX 630 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North America. |
|||
Compressive Strength | 360 MPa | 52200 psi | ISO 604 |
Vyncolit W5000 Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral filled. Excellent dimensional stability and very low coefficient of linear expansion and excellent chemical resistance at elevated temperatures in severa.. |
|||
Compressive Strength | 360 MPa | 52200 psi | ISO 604 |
Vyncolit X655/1 Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral filled. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in particular in the ABS system.. |
|||
Compressive Strength | 360 MPa | 52200 psi | ISO 604 |
Vyncolit X655RB Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral reinforced. Grade with superior stiffness, high dimensional stability and high wear resistance. Good chemical resistance against several fuels at elevate.. |
|||
Compressive Strength | 360 MPa @Treatment Temp. 200 °C, Time 3600 sec |
52200 psi @Treatment Temp. 392 °F, Time 1.00 hour |
ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |