Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 3650 MPa | 529000 psi | |
McDanel Advanced Ceramics 99.8% Alumina Information provided by McDanel Advanced Ceramic Technologies |
|||
Compressive Strength | 3650 MPa @Temperature 20.0 °C |
529000 psi @Temperature 68.0 °F |
|
Zircar Ceramics Alumina Furnaceware ZIRCAR Ceramics Alumina Furnaceware are high purity fully dense, fine grain aluminum oxide products suitable for use in applications with temperatures as high as 1800°C. Such uses include crucibles.. |