Polymer Property : Compressive Strength = 38600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 266 MPa
38600 psi
BCC Products BC 5010 Epoxy Laminating System
BC 5010 is a high quality, low viscosity room temperature curing laminating resin. A Safety System for the production of a variety of dimensionally stable fiberglass tools. BC 5010 features low odor..