Polymer Property : Compressive Strength = 40.6 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.280 MPa
40.6 psi
to 10% deformation
Pyrotek M-14 Compressible/Insulating Boards
ApplicationsSiphon gaskets Trough and ladle linings Tundishes Mill board substitute AdvantagesResistant to chemical attack Excellent thermal shock resistance Slightly flexible Moderately compressibl..