Mechanical Properties Metric English Comments
Compressive Strength 400 MPa

@Temperature 23.9 °C
58000 psi

@Temperature 75.0 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f..
Compressive Strength 400 MPa
58000 psi
Pyrotek TS-180 Thermoset Electrical Insulation Product
Glass reinforcement, Epoxy Resin, Straw Color. Excellent mechanical and electrical properties at elevated temperature.Information provided by Pyrotek.
Compressive Strength 400 MPa
58000 psi
Pyrotek TS-450 Thermoset Electrical Insulation Product
Glass reinforcement, Mica resin, Silver color. Highest temperature resistance. High dielectric properties.Information provided by Pyrotek.
Compressive Strength 400 MPa

@Treatment Temp. 250 °C,
Time 3600 sec
58000 psi

@Treatment Temp. 482 °F,
Time 1.00 hour
ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet
High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr..
Compressive Strength 400 MPa

@Treatment Temp. 150 °C,
Time 3600 sec
58000 psi

@Treatment Temp. 302 °F,
Time 1.00 hour
ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t..
Compressive Strength 400 MPa

@Temperature 23.0 °C
58000 psi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT 1101 Polyimide (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Compressive Strength >= 400 MPa
>= 58000 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet