Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 41.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 41.4 MPa
6000 psi
Ultimate; TM R050-38
Resinlab® EP1121-4 Adhesive / Casting Resin
Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives ..
Compressive Strength 41.4 MPa
6000 psi
Ultimate; TM R050-38
Resinlab® EP1225 Black Unfilled Epoxy Adhesive
Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil..
Compressive Strength 41.4 MPa
6000 psi
Break; TM R050-38
Resinlab® EP1225 Black Unfilled Epoxy Adhesive
Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil..
Compressive Strength 41.4 MPa
6000 psi
cured at 649°C
Pyrotek Pyrocast AR Castable Refractory
Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyro..
Compressive Strength 41.4 MPa
6000 psi
0.1% Offset; ASTM D695
Saint-Gobain Meldin® 7003 Isostatically Molded Bearing Grade MoS2 Filled Polyimide
Melidin® 7003 is a thermosetting polyimide that includes 15% molybdenum disulfide self-lubricating filler for wear applications that operate in a vacuum or in very dry conditions. Meldin® 700..
Compressive Strength 41.4 MPa
6000 psi
0.1 % Offset; ASTM D695
Saint-Gobain Meldin® 7022 Isostatically Molded Graphite Filled Polyimide
Finished parts and basic shapes made from 40% by weight graphite filled polyimide material for applications requiring a low coefficient of thermal expansion, self lubricating properties, and good di..
Compressive Strength 41.4 MPa
6000 psi
Cotronics Resbond™ 904 Ultra Temp Zirconia Adhesive and Coating
Ultra Temp 904 is a smooth creamy paste that is easily brushed on ceramics, graphite, metals, etc. to form adhesive bonds and coatings that will withstand 4000°F (2200°C) continuous heat. It has ..
Compressive Strength 41.4 MPa
6000 psi
3M H50/10000EPX Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Compressive Strength 41.4 MPa
6000 psi
3M HGS6000 Glass Bubbles
3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of..
Compressive Strength 41.4 MPa
6000 psi
3M K46 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Compressive Strength 41.4 MPa
6000 psi
ASTM D695
3M Scotchkote™ LW 405 Epoxy Concrete Mortar
Scotchkote Epoxy Concrete Mortar LW 405 has been specifically developed as a three component 100% solids light weight repair mortar for use on concrete surfaces.Product Features:Designed for applica..
Compressive Strength 41.4 MPa
6000 psi
Break; TM R050-38
Resinlab® EP1200LV Casting Resin
Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility an..
Compressive Strength 41.4 MPa
6000 psi
Break; TM R050-38
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin
Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro..