Polymer Property : Compressive Strength = 421000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 2900 MPa
421000 psi
ASTM C773
CoorsTek Zirconia-Toughened Alumina, ZTA
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Compressive Strength 2900 MPa
421000 psi
Aremco AREMCOLOX™ 502-1900-ZTA Dense Zirconia-Toughened Aluminum Oxide
This grade is made up of > 80% alumina and the balance yttria stabilized zirconia (Y-TZP). Provides some of the advantages of pure Y-TZP at a reduced price. The addition of zirconia increases greatl..