Mechanical Properties Metric English Comments
Compressive Strength 30.0 MPa

@Time 3.60e+7 sec
4350 psi

@Time 10000 hour
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: ..
Compressive Strength 30.0 MPa

@Strain 3.50 %
4350 psi

@Strain 3.50 %
DIN EN ISO 604
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: ..
Compressive Strength 30.0 MPa

@Time 3.60e+7 sec
4350 psi

@Time 10000 hour
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced
Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv..
Compressive Strength 30.0 MPa
4350 psi
Cold Crushing Strength
Chosun Refractories A23H Magnesia Carbon Bricks for Electric Arc Furnace
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 30.0 MPa

@Temperature 23.0 °C
4350 psi

@Temperature 73.4 °F
Elisto THERMOSTAR® MD 80 Pattern material
Block materialInformation provided by elisto