Mechanical Properties Metric English Comments
Compressive Strength 44.0 MPa

@Temperature 23.0 °C
6380 psi

@Temperature 73.4 °F
ASTM D695
DuPont Performance Polymers VESPEL TP-8311 Polyimide
Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in both dry and lubricated high temperature environmentsInformation provided b..