Polymer Property : Compressive Strength = 4550 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 31.4 MPa
4550 psi
Fired at Service temp. of 800°C, Cold Crushing
Sharadaa Ceramics REFINSUL ZAP-021 Insulating Castables
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l..
Compressive Strength 31.4 MPa
4550 psi
Cold Crushing Strength
Chosun Refractories CRMG-S02 Long Stopper
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 31.4 MPa
4550 psi
1% deformation; ASTM D695
Beijing Ranger Chem BLUESTAR® BS450 Acetal Copolymer
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Compressive Strength 31.4 MPa
4550 psi
1% deformation; ASTM D695
Beijing Ranger Chem BLUESTAR® BS350 Acetal Copolymer
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..