Polymer Property : Compressive Strength = 5.17 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 5.17 MPa
750 psi
Maximum working pressure
Potters Industries Q-Cel® 6028
Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat..
Compressive Strength <= 5.17 MPa
<= 750 psi
Isostatic working pressure
Potters Industries Q-Cel® 7023S Hollow Engineered Glass Microspheres
Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me..
Compressive Strength <= 5.17 MPa
<= 750 psi
Working pressure
Potters Industries Sphericel® 25P45 Hollow Engineered Glass Microspheres
Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength..
Compressive Strength 5.17 MPa
750 psi
3M K25 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..