Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 3.92 MPa | 569 psi | Cold Crushing |
Sharadaa Ceramics 60LBD Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Compressive Strength | 3.92 MPa | 569 psi | Dried at 110°C, Cold Crushing |
Sharadaa Ceramics REFINSUL ZAP-017 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Compressive Strength | 3.92 MPa | 569 psi | Fired at Service temp. of 1300°C, Cold Crushing |
Sharadaa Ceramics REFINSUL ZAP-017 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Compressive Strength | 3.92 MPa | 569 psi | Fired at 800°C, Cold Crushing |
Sharadaa Ceramics REFINSUL ZAP-019 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Compressive Strength | <= 3.92 MPa | <= 569 psi | Cold Crushing Strength |
Chosun Refractories HL-15 Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |