Polymer Property : Compressive Strength = 57.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 57.2 MPa
8300 psi
BCC Products Kwik Kast BC 8002 Urethane Casting
Kwik Kast II is an enhanced fast cast polyurethane tooling system. It has been reinvented for greater moisture resistance and improved filler suspension for easier premixing of the components. Kwik..