Mechanical Properties Metric English Comments
Compressive Strength 6.37 - 6.86 MPa
925 - 996 psi
1% Deformation; ASTM D695
Polikim EFALON® C-25 PTFE, 25% Glass Filled
C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings..