Polymer Property : Compressive Strength = 619 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 619 MPa
89800 psi
ASTM C-773-88 / DIN 51067T1
CeramTec 665 Steatite, MgO•SiO2
Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. 665 L533C has low dielectric loss. It makes exc..