Polymer Property : Compressive Strength = 62400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 430 MPa

@Treatment Temp. 200 °C,
Time 3600 sec
62400 psi

@Treatment Temp. 392 °F,
Time 1.00 hour
ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet
High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr..
Compressive Strength >= 430 MPa
>= 62400 psi
Ambient
China-Yixing Longly Refractories Tube SiC
SiC tube made by our company have lots of superior performance, such as high refractoriness, good wear and corrosion resistance, hardness, strength, thermal conductivity, thermal shock stability, as..