Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.448 MPa | 65.0 psi | 10% Deformation; Green |
Unifrax Fiberfrax® Duraboard® 500ES Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |
|||
Compressive Strength | 0.448 MPa | 65.0 psi | Compression Deflection, Value given for 12.7 mm/min, 25% deflection.; ASTM D3574 Test C |