Mechanical Properties Metric English Comments
Compressive Strength 45.0 MPa
6530 psi
Cold Crushing Strength
Gouda Vuurvast A 1 S Dense Refractory Brick
Description: A brick with a high creep resistance, successfully applied in anode baking furnaces and in the transition zone of rotary cement kilns.Remarks: This data represents average values, obtai..
Compressive Strength 45.0 MPa
6530 psi
Cold Crushing Strength
Gouda Vuurvast AK 44 Dense Refractory Brick
Description: A very dense, high duty fireclay brick with low iron and alkali content. Widely used in anode-baking furnaces (aluminum industry) and as the lining of the top of blast furnaces.Remarks:..
Compressive Strength 45.0 MPa
6530 psi
10% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Conditioned
Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 45.0 MPa
6530 psi
10% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Dry
Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 45.0 MPa

@Time 3.60e+7 sec
6530 psi

@Time 10000 hour
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced
Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed..
Compressive Strength 45.0 MPa
6530 psi
Practical Use (Water Absorption 1.8%); ASTM-D695
Toyobo GLAMIDE® T-422VOR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Compressive Strength 45.0 MPa

@Temperature 23.0 °C
6530 psi

@Temperature 73.4 °F
ASTM D695
DuPont Performance Polymers VESPEL TP-8549 Polyimide
Thermoplastic parts from filled PI (polyimide) for high mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Performance..
Compressive Strength 45.0 MPa
6530 psi
Cold Crushing Strength
Chosun Refractories ASC-1 Alumina Silicon Carbide Carbon Bricks for Torpedo Car
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 45.0 MPa
6530 psi
Cold Crushing Strength
Gouda Vuurvast AK 45 Dense Refractory Brick
Description: High quality refractory brick with a good volume stability up to 1450°C. Used where high load bearing capacities are required e.g. blast furnace stoves.Remarks: This data represents av..