Polymer Property : Compressive Strength = 688 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 688 MPa
99800 psi
ASTM C-773-88 / DIN 51067T1
CeramTec 192/193 Titania
192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra..