Polymer Property : Compressive Strength = 70.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 70.3 MPa
10200 psi
Tra-Con Tra-Bond FS12 Fast Cure Epoxy Adhesive System
TRA-BOND FS12 is an epoxy resin formulation developed for room temperature bonding applications where a fast cure epoxy adhesive is needed. This effective epoxy formulation consists of 100% reactive..
Compressive Strength 70.3 MPa
10200 psi
Aremco Ceramacastâ„¢ 576-N High Temperature Potting & Casting Alumina
Medium grain castable ceramic for large high temperature potting and tooling. Aremco offers a range of ceramic-based materials used for the assembly of high temperature, high power electrical devic..