Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 73.5 MPa | 10700 psi | Cold Crushing Strength |
Chosun Refractories GPB-2 Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |