Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 75.84 - 103.4 MPa | 11000 - 15000 psi | after 816°C |
Pyrotek Pyrocast ZG Refractory Shapes Aggregate Base: FireclayApplicationsDoor sill Door lintel Door jamb Information provided by Pyrotek. |
|||
Compressive Strength | 75.84 MPa | 11000 psi | Service Pressure |
Trelleborg AEM Eccofloat® EL-36/7300 Syntactic Foam EL Grade epoxy syntactic foams are the material of choice for manufacturing manned and unmanned submersibles because of their density range and ability to withstand exposure to diesel fuels and hydr.. |