Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 39.2 - 58.8 MPa | 5690 - 8530 psi | Cold Crushing |
Sharadaa Ceramics HA 70 High Alumina Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |