Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 67.0 MPa | 9720 psi | 20% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 307 Cast Polyamide 6, Heat Stabilized, Conditioned Application: slippers, inserts for coupling boxesInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 67.0 MPa | 9720 psi | 20% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 307 Cast Polyamide 6, Heat Stabilized, Dry Application: slippers, inserts for coupling boxesInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 67.0 MPa @Time 360000 sec |
9720 psi @Time 100 hour |
|
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |