Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 9960 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 68.6 MPa
9960 psi
Cold Crushing
Sharadaa Ceramics PCF40 Precast Prefired Brick
Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin..
Compressive Strength 68.6 MPa
9960 psi
Cold Crushing Strength
Chosun Refractories AH-4 Acid-Proof and Heat-Resistant Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 68.6 MPa
9960 psi
Cold Crushing Strength
Chosun Refractories AH-5 Acid-Proof and Heat-Resistant Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength <= 68.6 MPa
<= 9960 psi
Cold Crushing Strength
Chosun Refractories CUN-669 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength <= 68.6 MPa
<= 9960 psi
Cold Crushing Strength
Chosun Refractories HAL-SNA Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 68.6 MPa
9960 psi
Cold Crushing Strength
Chosun Refractories HSC-16HW Casting Block
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 68.6 MPa
9960 psi
Cold Crushing Strength
Chosun Refractories KSB-A65 Special Casting Block
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 68.6 MPa
9960 psi
Cold Crushing Strength
Chosun Refractories SAL70 Special Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 68.6 MPa
9960 psi
Cold Crushing Strength
Chosun Refractories SAL75 Special Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 68.6 MPa
9960 psi
Cold Crushing Strength
Chosun Refractories SC40 Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 68.6 MPa
9960 psi
Cold Crushing Strength
Chosun Refractories SF35 Hard Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).