Polymer Property : Izod Impact Unnotched = 140 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 190 J
140 ft-lb
Oil Quenched from 816°C; 430°C Temper Temperature
Latrobe LSS™ O1 Tool Steel (ASTM O1)
TLS O1 tool steel is the original oil-hardening, "non-shrinking" tool steel that can be hardened to the Rockwell C 65 range from a low austenitizing temperature. TLS O1 is a general-purpose tool ste..