Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 20.3 J | 15.0 ft-lb | Air Cooled from 1010°C; 593°C Temper Temperature |
Latrobe LSSâ„¢ 420 HC High Carbon Stainless Steel TLS 420 HC is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 55 HRC and good wear resistance. TLS 420 HC should be considered for applications such .. |
|||
Izod Impact Unnotched | 20.3 J | 15.0 ft-lb | Air Cooled from 1010°C; 593°C Temper Temperature |
Latrobe LSSâ„¢ 420 MQ Plastic Mold Steel (AISI 420) TLS 420 MQ is a highly-refined, Mold Quality stainless steel that is engineered to exhibit excellent polishability, good corrosion resistance, and good wear resistance. TLS 420 MQ is melted using an.. |
|||
Izod Impact Unnotched | 20.3 J | 15.0 ft-lb | Air Cooled from 1010°C; 593°C Temper Temperature |
Latrobe LSSâ„¢ 420 Supreme Plastic Mold Steel (AISI 420) TLS 420 Supreme is a specially-refined, mold-quality stainless steel that is engineered to provide supreme polishability, good corrosion resistance, and good wear resistance. TLS 420 supreme is manu.. |
|||
Izod Impact Unnotched | 20.3 J | 15.0 ft-lb | Oil Quenched from 954°C; As Quenched |
Latrobe LSSâ„¢ D3 Tool Steel (ASTM D3) TLS D3 tool steel is a high-carbon, high-chromium, oil-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, large, chromium-rich alloy carbides in the mi.. |
|||
Izod Impact Unnotched | 20.3 J | 15.0 ft-lb | Oil Quenched at 1238°C; 622°C Temper Temperature |
Latrobe Dynavanâ„¢ ASTM T15 Super High Speed Steel DYNAVAN (T15) is a super high speed steel designed for extra-high wear resistance and superior hot hardness. These properties result from the high carbon and vanadium contents which produce numerous.. |