Mechanical Properties Metric English Comments
Izod Impact Unnotched 21.7 J
16.0 ft-lb
Air Cooled from 1038°C; As Quenched
Latrobe LSSâ„¢ D7 Tool Steel (ASTM D7)
TLS D7 tool steel is a high-carbon, high-chromium air-hardening tool steel that exhibits exceptional wear resistance. The high carbon and vanadium contents result in numerous, hard vanadium carbide ..