Mechanical Properties Metric English Comments
Izod Impact Unnotched 28.5 J
21.0 ft-lb
Oil Quenched at 1204°C; 510°C Temper Temperature
Latrobe Corsairâ„¢ ASTM M3-1 High Speed Steel
CORSAIR (M3-1) contains carbon and vanadium levels that are intermediate between those of Double Six (M2) and Crusader (M3-2). This gives the steel a fine balance of wear resistance and grindability..
Izod Impact Unnotched 28.5 J
21.0 ft-lb
Oil Quenched at 1218°C; 482°C Temper Temperature
Latrobe Tatmo-VN™ ASTM M7 High Speed Steel
TATMO-VN is an M7 type high speed steel modified by alloy balancing and a nitrogen addition to develop superior hardness response in heat treatment. It is an excellent grade for many cutting tool ap..