Mechanical Properties Metric English Comments
Izod Impact Unnotched 43.4 J
32.0 ft-lb
Oil Quenched at 1177°C; 482°C Temper Temperature
Latrobe HS-29XLâ„¢ ASTM M2-HC High Speed Steel
HS-29XL (M2-HC) is the M2 composition with the carbon content increased and with the addition of alloy sulfides. The higher carbon content provides higher hardness and superior red hardness compared..
Izod Impact Unnotched 43.4 J
32.0 ft-lb
Oil Quenched at 1177°C; 482°C Temper Temperature
Latrobe Corsairâ„¢ ASTM M3-1 High Speed Steel
CORSAIR (M3-1) contains carbon and vanadium levels that are intermediate between those of Double Six (M2) and Crusader (M3-2). This gives the steel a fine balance of wear resistance and grindability..