Izod Impact Unnotched 47.0 J
34.7 ft-lb
when tempered at 900°F
Carpenter Four Star High Speed Steel Red-Wear® (AISI M4)
Carpenter Four Star, a molybdenum-tungsten high speed tool steel possessing high carbon and vanadium contents, provides a very high degree of wear resistance coupled with high strength.Applications:..