Polymer Property : Izod Impact Unnotched = 36.6 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 36.6 J
27.0 ft-lb
Oil Quenched at 1204°C; 622°C Temper Temperature
Latrobe Crusaderâ„¢ ASTM M3-2 High Speed Steel
CRUSADER (M3-2) is a high speed steel with an outstanding balance of red hardness, edge toughness and wear resistance. The additional carbon and vanadium provide good resistance to abrasion and edge..
Izod Impact Unnotched 36.6 J
27.0 ft-lb
Oil Quenched at 1121°C; 482°C Temper Temperature
Latrobe CM-50â„¢ ASTM M50 High Speed Steel
CM-50 is classified as an intermediate type high speed steel of the molybdenum chromium- vanadium variety. It is recommended for applications with moderate cutting conditions, such as woodworking to..
Izod Impact Unnotched 36.6 J
27.0 ft-lb
Oil Quenched at 1218°C; 622°C Temper Temperature
Latrobe Tatmo-VN™ ASTM M7 High Speed Steel
TATMO-VN is an M7 type high speed steel modified by alloy balancing and a nitrogen addition to develop superior hardness response in heat treatment. It is an excellent grade for many cutting tool ap..