Mechanical Properties Metric English Comments
Izod Impact Unnotched 32.5 - 42.0 J
24.0 - 31.0 ft-lb
Carpenter Micro-Melt® M-3 Class 2 Alloy (AISI M3)
Micro-Melt® M-3 Class 2 alloy is a powder metal tungsten-molybdenum high-speed steel possessing the superior wear resistance characteristics required for difficult cutting operations. The advantage..