Mechanical Properties Metric English Comments
Izod Impact Unnotched 84.0 J

@Thickness 12.7 mm
62.0 ft-lb

@Thickness 0.500 in
plate, solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 1.6 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Izod Impact Unnotched 84.0 J

@Thickness 12.7 mm
62.0 ft-lb

@Thickness 0.500 in
plate solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 12.7 mm (1/2 in.) thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Izod Impact Unnotched 84.0 J

@Thickness 12.7 mm
62.0 ft-lb

@Thickness 0.500 in
plate, solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 15.9 mm thick bar
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Izod Impact Unnotched 84.0 J

@Thickness 12.7 mm
62.0 ft-lb

@Thickness 0.500 in
plate, solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.0 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Izod Impact Unnotched 84.0 J

@Thickness 12.7 mm
62.0 ft-lb

@Thickness 0.500 in
plate solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.7 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Izod Impact Unnotched 84.0 J

@Thickness 12.7 mm
62.0 ft-lb

@Thickness 0.500 in
plate, solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Izod Impact Unnotched 84.0 J

@Thickness 12.7 mm
62.0 ft-lb

@Thickness 0.500 in
plate solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Izod Impact Unnotched 84.0 J

@Thickness 12.7 mm
62.0 ft-lb

@Thickness 0.500 in
plate, solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate, aged 3 hours at 816°C
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Izod Impact Unnotched 84.0 J

@Thickness 12.7 mm
62.0 ft-lb

@Thickness 0.500 in
plate, solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 4.8 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Izod Impact Unnotched 84.0 J

@Thickness 12.7 mm
62.0 ft-lb

@Thickness 0.500 in
plate, solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 7.9 mm thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Izod Impact Unnotched 84.0 J

@Thickness 12.7 mm
62.0 ft-lb

@Thickness 0.500 in
plate solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 7.9 mm thick plate, aged 3 hours at 816°C
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Izod Impact Unnotched 84.0 J

@Thickness 12.7 mm
62.0 ft-lb

@Thickness 0.500 in
plate, solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 3.2 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Izod Impact Unnotched 84.0 J

@Thickness 12.7 mm
62.0 ft-lb

@Thickness 0.500 in
plate solution heat-treated at 1232°C (2250°F), air cooled, tested at RT.
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate, aged 3 hours at 816°C
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..