Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 119 J | 88.0 ft-lb | Air Cooled from 1010°C; 593°C Temper Temperature |
Latrobe LSSâ„¢ D5 Tool Steel (ASTM D5) TLS D5 tool steel is an air hardening, high-carbon, high-chromium, tool steel that is characterized by a cobalt addition which provides unique resistance to galling and pick-up. The cobalt also impa.. |