Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 1.00 J @Temperature -30.0 °C |
0.738 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Prevex VFAX PPE+PS High impact strength. 180F (82C) HDT. Improved productivity/reliability.This data was supplied by SABIC-IP for the Americas region. |