Polymer Property : Impact Test = 1.10 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 1.10 J

@Temperature -40.0 °C
0.811 ft-lb

@Temperature -40.0 °F
ASTM D3763
Diamond Polymers Centrex® HGM Automotive Grade, Injection Molding Grade
Centrex HGM resin is an exceptionally high-gloss grade of ASA (acrylonitrile-styrene-acrylate). This injection molding grade has excellent gloss retention, excellent resistance to chemicals and high..