Polymer Property : Impact Test = 1.60 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 1.60 J

@Temperature 23.0 °C
1.18 ft-lb

@Temperature 73.4 °F
Multi-axial, at max. load; ASTM D3763
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (1.5 mm Molded Thickness)
AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Impact Test 1.60 J

@Temperature 23.0 °C
1.18 ft-lb

@Temperature 73.4 °F
Multi-axial, at max. load; ASTM D3763
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (1.5 mm Molded Thickness)
AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Impact Test 1.60 J

@Temperature 23.0 °C
1.18 ft-lb

@Temperature 73.4 °F
Multi-axial, at max. load; ASTM D3763
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness)
AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..