Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 100 J @Thickness 3.17 mm, Temperature -40.0 °C |
74.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM |
ExxonMobil Paxon™ 7003 Crosslinkable Rotational Molding Resin Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite.. |
|||
Impact Test | 100 J @Thickness 3.17 mm, Temperature -40.0 °C |
74.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM |
ExxonMobil Paxon™ 7004 Crosslinkable Rotational Molding Resin Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite.. |
|||
Impact Test | 100 J @Thickness 3.17 mm, Temperature -40.0 °C |
74.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM |
ExxonMobil Paxon™ 7203 Crosslinkable Rotational Molding Resin Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite.. |
|||
Impact Test | 100 J @Thickness 3.17 mm, Temperature -40.0 °C |
74.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM |
ExxonMobil Paxon™ 7204 Crosslinkable Rotational Molding Resin Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite.. |
|||
Impact Test | 100 J @Thickness 4.00 mm |
73.8 ft-lb @Thickness 0.157 in |
Multi-axial, total energy; ISO 6603-2 |
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This.. |