Impact Test 105 J

@Thickness 6.34 mm,
Temperature -40.0 °C
77.4 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
Braskem RC35U4 LLDPE Rotomolding Polyethylene
The resin RC35U4 is a linear low-density polyethylene, 1-butene based, with high stiffness and an adequate balance of processability and environmental stress cracking resistance. It contains long te..